HOME
Trimet
 

EN AB-44400   << back

Chemical designation: EN AB-AlSi9
Previous Swedish standard: Type 4255
 
Chemical composition:  
  Min % Max %
 Si 8,0 11,0
 Fe - 0,55
 Cu - 0,08
 Mn - 0,50
 Mg - 0,10
 Cr - -
 Ni - 0,05
 Zn - 0,15
 Pb - 0,05
 Sn - 0,05
 Ti - 0,15
General description of properties:
Near-eutectic alloy with excellent castability, but likely to adhere to the tool. Good resistance to hot tearing and high resistance to chemical attack.

Suitable applications:
For castings that must have good toughness and resistance to corrosion.

Heat treatment:

Not age hardenable
Others each max 0,05%
and total max 0,15%
 

Casting characteristics, S-Sand cast, K-Chill cast:
Solidification
range, ºC, about
Casting
temperature
ºC, about
 Fluidity Resistance to hot
tearing
Shrinkage
%, about
Pressure
tightness
600-550 650-700 Excellent Excellent 0,5 - 0,8  Good

Mechanical properties of separately untreated cast test bars:
Tensile strength,
Rm, MPa, min.
Proof stress
Rp0,2, MPa, min.
Elongation
A50, %, min.
Brinell hardness
HBS, min.
220 120 2 55

Mechanical and physical properties:
Density
Kg/Dm³
Strength Machinability Weldability Resistance to
corrosion
2,65 Satisfact. Satisfact. Poor Satisfact.
 
Decorative
anodizing
Ability to be
polished
Linear thermal
expansion
293-373ºK, ºK¯¹
Electrical
conductivity
MS/m
Thermal
conductivity
W/mºK
Not recom. Poor 21 x 10¯6 16 – 22 130 - 150
 